ADG - Pneumatic Dross Grabber

ADG - Pneumatic Dross Grabber

Removing Dross Without Losing Zinc

Dross - the zinc-iron intermetallic that settles at the bottom of a galvanizing kettle - must be removed regularly. Left in place, it degrades coating quality, causes rough finishes, and reduces effective bath volume. Manual removal is slow, exposes operators to molten zinc at 450–600°C, and typically drags out far more free zinc than dross.

The AURO ADG is a pneumatically operated clamshell grab designed to lift dross cleanly from the kettle floor while returning free zinc to the bath. It is built for deep kettles and removes the operator from direct proximity to the molten surface.

Design

Perforated Clamshell - Zinc Stays in the Bath

Both grab flaps are perforated with sized holes. As the bucket clears the surface, free molten zinc drains straight back into the kettle while the dross is retained.

Non-Forced Closure

The closure mechanism does not force shut against an obstruction. If a lost part or foreign object is caught between the flaps, the bucket will not crush it and the grab structure is not damaged. This protects both the equipment and any workpiece that has been dropped in the kettle.

Deep Kettle Geometry

The frame is sized to the customer's kettle dimensions. Reach, flap span, and structural proportions are built to order rather than adapted from a standard unit - which matters on deep kettles where a generic grab cannot reach the floor corners where dross accumulates.

Materials

All submerged parts are fabricated in stainless steel. A heat shield protects the pneumatic actuator and control lines from radiant heat.